A Comparison of the Adaptive Response of Staphylococcus aureus vs. Streptococcus mutans and the Development of Chlorhexidine Resistance

\r\nMarieke van de Lagemaat&#x;Marieke van de Lagemaat1†Valerie Stockbroekx&#x;Valerie Stockbroekx1†Gsinda I. Geertsema-DoornbuschGésinda I. Geertsema-Doornbusch2Melissa DijkMelissa Dijk1Vera CarnielloVera Carniello2Willem WoudstraWillem Woudstra2Henny C. van der Mei*Henny C. van der Mei2*Henk J. BusscherHenk J. Busscher2Yijin RenYijin Ren1
  • 1University of Groningen and University Medical Center Groningen, Department of Orthodontics, Groningen, Netherlands
  • 2University of Groningen and University Medical Center Groningen, Department of Biomedical Engineering, Groningen, Netherlands

Antimicrobials with nonselective antibacterial efficacy such as chlorhexidine can be effective in reducing biofilm, but bear the risk of inducing resistance in specific bacteria. In clinical practice, bacteria such as Staphylococcus aureus have been found resistant to chlorhexidine, but other bacteria, including Streptococcus mutans, have largely remained susceptible to chlorhexidine despite its widespread use in oral healthcare. Here, we aim to forward a possible reason as to why S. aureus can acquire resistance against chlorhexidine, while S. mutans remains susceptible to chlorhexidine. Measurement of surface-enhanced fluorescence indicated that chlorhexidine caused gradual, but irreversible deformation to adhering green fluorescent S. aureus due to irreparable damage to the cell wall. Concurrently, the metabolic activity of adhering staphylococci was higher than of planktonic bacteria, suggesting efflux mechanisms may have been activated upon cell wall deformation, impeding the buildup of a high chlorhexidine concentration in the cytoplasm and therewith stimulating the development of chlorhexidine resistance in S. aureus. Exposure of S. mutans to chlorhexidine caused immediate, but reversible deformation in adhering streptococci, indicative of rapid self-repair of cell wall damage done by chlorhexidine. Due to cell wall self-repair, S. mutans will be unable to effectively reduce the chlorhexidine concentration in the cytoplasm causing solidification of the cytoplasm. In line, no increased metabolic activity was observed in S. mutans during exposure to chlorhexidine. Therewith, self-repair is suicidal and prevents the development of a chlorhexidine-resistant progeny in S. mutans.

Introduction

The increasing resistance of bacteria to antimicrobials occurring over the past decades has become a major concern for public health (Howard et al., 2003; Roca et al., 2015; World Health Organization [WHO], 2018). Due to the increase in antimicrobial resistance among different bacterial strains, it is predicted that in 2050, antimicrobial-resistant infections will be the main cause of death (O’Neill, 2014). Chlorhexidine is a broad-spectrum antimicrobial and widely used in healthcare settings as a disinfectant for the skin, hands, and in oral healthcare products (Zhang et al., 2013; Okada et al., 2016). Chlorhexidine carries positively-charged groups that can bind to negatively-charged bacterial cell surfaces (Cieplik et al., 2019) to cause cell wall damage and catastrophic leakage of intracellular material. Mild cell wall damage and leakage of intracellular material will not cause immediate cell death. Instead, mild cell wall damage will yield loss of intracellular pressure, which is accompanied by minor cell wall deformation in adhering bacteria (Carniello et al., 2020). Bacterial cell wall deformation is only demonstrable using highly sensitive methods such as atomic force microscopy (Zuttion et al., 2020) or surface-enhanced fluorescence (Lee et al., 2011; Li et al., 2014; Carniello et al., 2018a). Severe, catastrophic cell wall damage will eventually result in bacterial death (Gilbert and Moore, 2005). These properties provide chlorhexidine with a broad-spectrum antimicrobial activity against both the Gram-positive and Gram-negative bacteria (Beyth et al., 2003). Chlorhexidine is considered safe for use in the oral cavity at appropriately low concentrations (Denton, 2001) and has become the “gold” standard in antibacterial mouthrinses (Balagopal and Arjunkumar, 2013).

Microbial resistance against chlorhexidine has long been considered rare if not impossible (Schlett et al., 2014; Saleem et al., 2016), but has recently been reported in Staphylococcus aureus, coagulase-negative staphylococci, Klebsiella pneumoniae, Pseudomonas aeruginosa, Acinetobacter baumannii, and Candida albicans. For these bacteria, the intensity of chlorhexidine use was found proportional with the development of resistance (Block and Furman, 2002). Importantly, after acquiring resistance to chlorhexidine, Acinetobacter spp., K. pneumoniae, and Pseudomonas spp. can develop cross-resistance to different antibiotics (Kampf, 2016). Horizontal gene transfer of chlorhexidine resistance at subminimal inhibitory concentrations of chlorhexidine has been reported in Escherichia coli (Jutkina et al., 2018). Exposure of P. aeruginosa to 4 μg/ml chlorhexidine caused downregulation of genes involved in membrane transport, oxidative phosphorylation, electron transport, and DNA repair, while multidrug efflux pump genes were upregulated (Nde et al., 2009).

Bacterial resistance against chlorhexidine in oral bacteria is still rare for reasons that have only been speculated upon. However, although chlorhexidine does not penetrate deeply in oral biofilms (Zaura-Arite et al., 2001), its prolonged substantive presence on oral soft tissues and low-level release (Reda et al., 2021) are ideal for developing resistance. Therefore, clinical use of chlorhexidine has been restricted to applications with clear patient benefits and elimination of its use in applications without healthcare benefits has been suggested (Kampf, 2016). While still being allowed for oral use, safeguarding the much-needed use of chlorhexidine for oral applications in absence of equally effective alternatives requires better understanding of why oral bacteria seem not to develop chlorhexidine resistance.

Therefore, we compare the response to chlorhexidine of S. aureus, a pathogen involved in a wide variety of clinical infections (McCormack et al., 2015) and Streptococcus mutans, a cariogenic oral pathogen (Loesche, 1986). First, nanoscopic deformation of the cell walls of both the strains, including a chlorhexidine-resistant S. aureus variant, was determined upon exposure to chlorhexidine using surface-enhanced fluorescence. Cell wall damage at the more microscopic, membrane level was studied after propidium iodide staining of chlorhexidine-exposed bacteria using fluorescence microscopy. Since maintenance of antimicrobial resistance is known to be energy-consuming, metabolic activity was monitored using 3-(4,5-dimethylthiazol-2-yl)-2,5-diphenyltetrazolium bromide (MTT) reduction assay during bacterial exposure to chlorhexidine. Based on the collective data obtained, a possible reason is forwarded through which S. aureus can readily develop resistance against chlorhexidine, while S. mutans remains susceptible to chlorhexidine.

Materials and Methods

Bacterial Strains, Growth Conditions, and Harvesting

In order to allow measurement of cell wall deformation using surface-enhanced fluorescence, two green fluorescent bacterial strains were selected. S. mutans UA159GFP (Deng et al., 2007) and S. aureus ATCC 12600GFP (Li et al., 2011) were grown on Todd Hewitt Broth (THB) (Oxoid, Basingstoke, United Kingdom) and Tryptone Soya Broth (TSB) (Oxoid, Basingstoke, United Kingdom) agar plates, respectively. THB agar plates were supplemented with 10 μg/ml erythromycin (Sigma-Aldrich, St Louis, MO, United States) and TSB agar plates were supplemented with 10 μg/ml tetracycline (Sigma-Aldrich, St. Louis, MO, United States). One colony of S. mutans was inoculated in THB supplemented with 10 μg/ml erythromycin and similarly for S. aureus in TSB supplemented with 10 μg/ml tetracycline. S. mutans UA159GFP was grown at 37°C with 5% CO2 and S. aureus was grown under aerobic conditions. After 24 h, these precultures were inoculated in 200 ml (1:20) THB for S. mutans and TSB for S. aureus without antibiotics and cultured for 16 h at 37°C, yielding early-stationary phase bacteria.

Bacterial cultures were harvested by centrifugation (5 min, 5,000 g, 10°C) and washed twice with a phosphate buffer (2 mM potassium phosphate, 50 mM KCl, and 1 mM CaCl2, pH 7.0). After washing, bacteria were resuspended in phosphate buffer with THB or TSB (30:1) to maintain metabolic activity. The bacterial suspension was sonicated (3 × 10 s, 30 W) in an ice-water bath (Vibra Cell Model 375, Sonics and Materials Incorporation, Danbury, CT, United States) and the bacteria were enumerated using a Bürker-Türk counting chamber and suspensions (3 × 108/ml) were diluted in phosphate buffer supplemented with THB or TSB (30:1) to a bacterial concentration, appropriate for the different experiments. All the experiments were done in triplicate with different bacterial cultures.

Minimal Inhibitory Concentration of Chlorhexidine

A commercial chlorhexidine mouthrinse (Curasept ADS 212, Curasept S.p.A., Saronno, Italy) containing 0.12% (1,200 μg/ml) chlorhexidine digluconate was used in this study. Bacteria were exposed to 2-fold serial dilutions (i.e., 9.6, 4.8, 2.4, 1.2, 0.6, and 0.3 μg/ml) of the mouthrinse in sterile water. 100 μl of different dilutions of the mouthrinse were added to 100 μl of a bacterial suspension (2 × 105/ml) in the appropriate growth medium in 96-well plates and incubated at 37°C for 24 h. After incubation, the minimal inhibitory concentration (MIC) was taken as the lowest chlorhexidine concentration at which no visible growth was observed.

Development of Chlorhexidine-Resistant Variants

For the development of chlorhexidine-resistant bacterial strains, precultures of S. mutans UA159GFP and S. aureus ATCC 12600GFP were diluted 1:100 in appropriate growth media and grown with chlorhexidine added at its MIC. Bacteria were subcultured daily at the same chlorhexidine concentration over 4 consecutive days. Culturable bacteria that remained present after 4 days were subsequently grown over another sequence of 4 consecutive days at a 0.3 μg/ml higher chlorhexidine concentration than in the previous sequence. MIC was measured daily during each sequence of 4 consecutive days. Subculturing was discontinued when a culture did not demonstrate any bacterial growth by visual inspection of the culture turbidity. In order to check whether prolonged culturing under chlorhexidine exposure affected bacterial fluorescence, fluorescence was monitored regularly on agar plates using an In Vivo Imaging System (IVIS, Lumina II, Caliper LifeScience, Hopkinton, MA, United States), with an excitation wavelength of 465 nm and emission in a range from 515 to 575 nm. Cultures after repeated growth in presence of chlorhexidine were stored in a −80°C freezer, with 7% dimethyl sulfoxide added.

Surface-Enhanced Fluorescence

Molecular fluorescence is enhanced when fluorescent molecules are in the close vicinity (<30 nm) of a metal surface (Lee et al., 2011). This phenomenon, called surface-enhanced fluorescence, can be applied to measure the small deformation that adhering fluorescent bacteria experience in response to the adhesion forces arising from a substratum surface (see Figure 1 for schematics). As a major advantage over atomic force microscopy, surface-enhanced fluorescence is more sensitive and measures over a larger population of bacteria, depending on the number of bacteria adhering to the metal surface.

FIGURE 1
www.frontiersin.org

Figure 1. Bacterial cell wall deformation upon adhesion of a fluorescent bacterium to a metal surface from its planktonic state; cell wall deformation will gradually increase under the influence of adhesion forces exerted by the substratum and bring more fluorophores (red color) within the cytoplasm closer to the metal surface within the range of surface enhancement [schematics taken from Carniello et al. (2018a) with permission from the Royal Society of Chemistry].

For surface-enhanced fluorescence, bacteria suspended in phosphate buffer supplemented with growth medium (30:1) were injected in a parallel plate flow chamber, with a glass top-plate and a polished, stainless steel bottom-plate. Fluorescence was measured using a bio-optical imaging system (see above). Images had a field of view of 7.5 cm × 7.5 cm, while exposure time was set at 10 s, employing a focal ratio of 1. Temperature throughout an experiment was maintained at 20°C. With the Living Image software package 3.1 (Caliper LifeScience), a user-defined region of interest was constructed in each image of 4.0 cm × 1.0 cm to calculate the average fluorescence radiance (photons s–1 cm–2 steradian–1).

Background fluorescence in the region of interest was measured in a flow chamber filled with phosphate buffer, supplemented with growth medium (30:1) in the absence of suspended bacteria. This background fluorescence radiance was subtracted from all the fluorescent radiances measured. Next, bacteria were injected into the flow chamber. Sedimentation of suspended bacteria and their adhesion was allowed in the absence of flow under the influence of gravity, while acquiring images every 15 min for 3 h, previously found sufficient for complete sedimentation of all the suspended bacteria (Li et al., 2014). Subsequently, the flow chamber was filled with 5 ml of the commercial chlorhexidine mouthrinse at different dilutions. Fluorescence image acquisition continued every 15 min for an additional 2 h. Phosphate buffer supplemented with growth medium (30:1) was used as a control.

Assuming even intracellular distribution of green fluorescent proteins, the increase in fluorescence radiance due to adhering bacteria relative to planktonic bacteria was expressed as total fluorescence enhancement (Li et al., 2014), according to:

TFE(t)=R(t)-R0R(0)-R0(1)

Where, R(t) is the fluorescence radiance at time t, R(0) is the fluorescence radiance measured for a planktonic suspension, and R0 is the fluorescence radiance of the background.

Bacterial Membrane Damage

To determine the percentage of damage upon chlorhexidine exposure to the cell membrane, as an integral part of the cell wall, bacteria were stained with red fluorescent propidium iodide (LIVE/DEAD BacLight Bacterial Viability, Thermo Fisher Scientific, Waltham, MA, United States). Propidium iodide is only able to enter bacteria with a damaged membrane (Lehtinen et al., 2004). Membrane damage was inflicted according to a similar protocol as in surface-enhanced fluorescence. After incubation with chlorhexidine, 15 μl of propidium iodide (20 mM) was added to each well. Fluorescence was imaged using a Leica DM4000B fluorescence microscope with a 40× water objective by taking three images of each well. While closing the red channel, green fluorescent bacteria were enumerated as a measure of the total number of bacteria in an image, while those bacteria also displaying red fluorescence were taken as membrane damaged (Lehtinen et al., 2004).

Metabolic Activity

The influence of the different concentrations of chlorhexidine on bacterial metabolic activity was determined with 3-(4,5-dimethylthiazol-2-yl)-2,5-diphenyltetrazolium bromide (MTT) reduction assay (Krom et al., 2007). After exposure to chlorhexidine according to a similar protocol as in surface-enhanced fluorescence, MTT solution (0.5 mg/ml thiazolyl blue tetrazolium bromide in phosphate buffer, 10 mg/ml glucose, and 0.1 mM menadione) was added to each well and left for 30 min at 37°C in the dark. After 30 min, wells were washed once with water and mixed with acid isopropanol (5% 1 M HCl in isopropanol) for 15 min. After 15 min, 100 μl of the suspension was removed and added to a new 96-wells plate and absorptions were measured at 560 nm with the FLUOstar Optima Microplate Reader (BMG Labtech, Offenburg, Germany). All the experiments were performed in triplicate with different bacterial cultures. The data were normalized with respect to the metabolic activity of the bacterial strains after 3 h adhesion, i.e., before chlorhexidine exposure.

Physicochemical Bacterial Cell Surface Characterization

To determine whether the physicochemical bacterial cell surface properties were affected by chlorhexidine exposure, microbial adhesion to hydrocarbons (kinetic MATH assay) and zeta potentials were measured as a function of exposure time of the bacteria to chlorhexidine dissolved in phosphate buffer. MATH was carried out as previously described (Lichtenberg et al., 1985). Briefly, bacteria were resuspended in 3 ml phosphate buffer (pH 7.0) supplemented with chlorhexidine and containing 20:1 hexadecane to an initial absorbance at 600 nm between 0.4 and 0.6. Initial absorbance at time zero ([A0]) was measured photospectrometrically (Spectronic 20 Genesys, Spectronic Instruments, Rochester, NY, United States). After vortexing, the suspension for 10 s, and settling of the bacteria for 10 min, absorbance was measured again at time t ([At]). This procedure was repeated five more times, to allow calculation of the initial rate of bacterial removal from the aqueous phase according to:

Rateofinitialremoval=limt0ddtlog(AtA0×100)(2)

where, t is vortexing time.

The charge properties of the bacterial surfaces were determined by measuring the electrophoretic mobility using a bacterial suspension (3 × 108 bacteria/ml) in phosphate buffer (pH 7.0) supplemented with chlorhexidine. Particulate microelectrophoresis was carried out on a Zetasizer Nano ZS (Malvern Instruments, Worcestershire, United Kingdom). Electrophoretic mobilities measured were converted into zeta potentials, employing the Helmholtz–Smoluchowski equation (Van der Wal et al., 1997).

Statistical Analysis

Data were statistically analyzed using the paired and two-tailed Student’s t-tests with Microsoft Excel 2010. Significance was established at p < 0.05.

Results

Induction of Chlorhexidine Resistance Upon Subculturing at Different Chlorhexidine Concentrations

Prior to chlorhexidine exposure, the MIC of both the S. mutans UA159GFP and S. aureus ATCC 12600GFP was 1.2 μg/ml. In order to induce chlorhexidine resistance, planktonic cultures of S. mutans UA159GFP and S. aureus ATCC 12600GFP were grown in medium, supplemented with chlorhexidine. After daily subculturing at increasing chlorhexidine concentrations starting at sub-MIC over 4 consecutive days, no culturable S. mutans was observed when the chlorhexidine concentration exceeded MIC (Supplementary Figure 1). For S. aureus, culturable staphylococci remained present after 13 repetitions of 4 day sequences of growth at stepwise increasing chlorhexidine concentrations, acquiring a MIC of 4.8 μg/ml, i.e., four times the starting MIC of S. aureus ATCC 12600GFP (Supplementary Figure 1). This resistant variant of S. aureus ATCC 12600GFP was subsequently used in further experiments.

Cell Wall Deformation in Adhering Staphylococcus aureus and Streptococcus mutans During Chlorhexidine Exposure

Both the chlorhexidine-susceptible S. aureus strain (Figure 2A) and its chlorhexidine-resistant variant (Figure 2B) demonstrated a gradual increase in total fluorescence enhancement during the first 3 h of sedimentation and adhesion from phosphate buffer to a stainless steel surface, indicative of cell wall deformation. After 3 h, total fluorescence enhancement remained constant for at least 6 h upon continued exposure to buffer. However, the resistant variant (Figure 2B) deformed faster and more extensively than the chlorhexidine-susceptible strain (Figure 2A). Total fluorescence enhancement of S. mutans during sedimentation and adhesion followed by continued exposure to phosphate buffer hovered around 1 for at least 6 h, indicating absence of cell wall deformation upon adhesion (Figure 2C). Continued exposure to different concentrations of chlorhexidine after sedimentation and adhesion in phosphate buffer led to a different response in staphylococci than in streptococci. Both the chlorhexidine-susceptible (Figure 2A) and chlorhexidine-resistant S. aureus (Figure 2B) demonstrated gradual increase in total fluorescence enhancement that was independent of chlorhexidine concentration. These increases in total fluorescence enhancement remained to increase for at least 6 h, indicative of permanent cell wall deformation. Cell wall deformation was significantly (p < 0.05, Student’s t-test) larger for the already weakened cell wall of the resistant variant (Figure 2B) as compared with its chlorhexidine-susceptible parent strain (Figure 2A). S. mutans, on the other hand, demonstrated a fast increase in total fluorescence enhancement upon chlorhexidine exposure (Figure 2C). The increase in total fluorescence enhancement was dependent on the chlorhexidine concentration during exposure and decreased gradually over time to the level observed in phosphate buffer without chlorhexidine added.

FIGURE 2
www.frontiersin.org

Figure 2. Cell wall deformation derived from total fluorescence enhancement (TFE) in Staphylococcus aureus and Streptococcus mutans adhering to stainless steel upon exposure to chlorhexidine. Stable cell wall deformation due to adhesion was first established in phosphate buffer supplemented with growth medium (30:1) during 3 h, after which chlorhexidine was added (see arrow). (A) TFE of S. aureus ATCC 12600GFP as a function of time for different chlorhexidine concentrations. (B) Same as panel a, now for S. aureus ATCC 12600GFP, made resistant to 4.8 μg/ml chlorhexidine. (C) Same as panel a, now for S. mutans UA159GFP. All the error bars represent SDs over triplicate measurements with different bacterial cultures.

The physicochemical surface properties, bacterial zeta potentials (Figure 3A), and hydrophobicities (Figure 3B) relevant for adhesion did not change upon chlorhexidine exposure for all the three strains.

FIGURE 3
www.frontiersin.org

Figure 3. Physicochemical cell surface properties of S. aureus and S. mutans upon exposure to chlorhexidine. (A) Zeta potentials of bacteria in phosphate buffer as a function of time during exposure to 1× minimal inhibitory concentration (MIC) chlorhexidine. (B) Initial removal rates of bacteria from phosphate buffer by hexadecane as a function of time during exposure to 1× MIC chlorhexidine. All the error bars represent SDs over triplicate measurements with different bacterial cultures.

Cell Wall Damage in Adhering Staphylococcus aureus and Streptococcus mutans Measured Using Fluorescence Staining

Cell wall weakening was further studied by assessing cell wall damage based on cell membrane permeability to red fluorescent propidium iodide. Damage to the membrane, as an integral part of the cell wall, can be demonstrated at microscopic level and over a large population of bacteria by staining with red fluorescent propidium iodide, entering only damaged cell walls with increased membrane permeability.

Exposure of adhering bacteria to different concentrations of chlorhexidine caused nearly 50% of S. aureus to become membrane damaged, irrespective of concentration (Figure 4A). In the chlorhexidine-resistant S. aureus variant, exposure to chlorhexidine led to significantly fewer bacteria with membrane damage (<25%) (Figure 4B). Very few S. mutans became membrane damaged upon exposure to chlorhexidine (Figure 4C). Collectively, these data suggest that S. mutans suffers considerably less cell wall damage upon exposure to chlorhexidine than the susceptible S. aureus strain (p < 0.05) and even less than a chlorhexidine-resistant S. aureus variant although initially upon exposure to chlorhexidine it deforms equally as staphylococci do.

FIGURE 4
www.frontiersin.org

Figure 4. Cell wall weakening as a result of membrane damage of S. aureus and S. mutans after 2 h exposure to chlorhexidine. (A) Percentage cell membrane damaged bacteria after exposure to different chlorhexidine concentrations for S. aureus ATCC 12600GFP. Cell membrane damage was inferred from red fluorescence after staining with propidium iodide. Total fluorescence prior to exposure to chlorhexidine was taken as 100%. (B) Same as panel a, now for S. aureus ATCC 12600GFP, made resistant to 4.8 μg/ml chlorhexidine. (C) Same as panel a, now for S. mutans UA159GFP. All the error bars represent SDs over triplicate measurements with different bacterial cultures.

Self-Repair of Cell Wall Damage Inflicted by Chlorhexidine

In order to verify the suggestion of self-repair, cell wall damage was inflicted upon both the strains by a short-term, 15 min exposure to 1.2 μg/ml chlorhexidine (MIC) and compared with the cell wall damages inflicted by longer-term, 2 h exposure. Short-term exposure to chlorhexidine yielded only 10% of the S. aureus bacteria to become cell wall damaged, while 99% of S. mutans was already cell wall damaged, allowing penetration of red fluorescent propidium iodide (Figure 5). Upon continued exposure to chlorhexidine up to 2 h, however, 38% of the S. aureus appeared cell wall damaged than upon short-term exposure, but almost the entire population (96%) of S. mutans within a microscopic field of view had fully self-repaired the damage over time. A sub-MIC concentration of chlorhexidine showed similar self-repair as observed at MIC (Supplementary Figure 2). This confirms the presence of a self-repair mechanism against cell wall damage inflicted by chlorhexidine in S. mutans that is absent in S. aureus. However, at chlorhexidine concentration far above MIC (600 μg/ml), self-repair in S. mutans was no longer observed (see also Supplementary Figure 2).

FIGURE 5
www.frontiersin.org

Figure 5. Self-repair in cell membrane damaged S. aureus and S. mutans upon 15 min or 2 h exposure to chlorhexidine. Cell membrane damaged bacteria after 15 min exposure to 1.2 μg/ml chlorhexidine and after 2 h exposure to 1.2 μg/ml chlorhexidine. Both the strains are green fluorescent, while red fluorescent bacteria are cell wall damaged as inferred from the penetration of red fluorescent propidium iodide through the damaged cell wall.

Metabolic Activity During Chlorhexidine Exposure to Adhering Staphylococcus aureus and Streptococcus mutans

Initially, short-term (15 min) exposure to 1.2 μg/ml chlorhexidine did not show an increase in metabolic activity (Figure 6) in the resistant S. aureus and in S. mutans, but a small increase in the susceptible S. aureus. Exposure to the lower chlorhexidine concentrations shows a small, but not significant increase in metabolic activity for the S. aureus strains as compared to buffer exposure. After 2 h exposure to chlorhexidine, the metabolic activity of both the S. aureus strains at 0.6 and 1.2 μg/ml was significantly (p < 0.05, Student’s t-test) higher than of the S. mutans strain. S. mutans exhibited no significant increased metabolic activity upon self-repair of chlorhexidine-inflicted cell wall damage (Figure 6).

FIGURE 6
www.frontiersin.org

Figure 6. Metabolic activity of adhering S. aureus and S. mutans upon growth in presence of different concentrations of chlorhexidine, expressed with respect to the metabolic activity measured just prior to chlorhexidine exposure. (A) Metabolic activity of the bacterial strains after exposure to chlorhexidine for 15 min. (B) Metabolic activity of the bacterial strains after exposure to chlorhexidine for 2 h. All the error bars represent SDs over triplicate measurements with different bacterial cultures.

Discussion

In this article, we speculated upon the question of why S. aureus strains can be found resistant to chlorhexidine, while other bacteria, most notably oral S. mutans, largely remain susceptible to chlorhexidine. The data presented here are in part derived from the measurement of cell wall deformation using surface-enhanced fluorescence, providing a never explored pathway to understand the different responses of S. aureus and S. mutans toward chlorhexidine. Collectively, the data indicate that chlorhexidine at low concentration (1.2 μg/ml), characteristic for the substantive release of chlorhexidine adsorbed to oral tissues (Kumar, 2017; Reda et al., 2021), causes irreparable damage to the S. aureus cell wall. At the same time, cell wall damage causes increased efflux of chlorhexidine, impeding the buildup of a high chlorhexidine concentration in the cytoplasm that might cause precipitation of proteins and nucleic acids. This efflux is accompanied by increased metabolic activity, suggesting activation of efflux pumps that may be involved in the development of chlorhexidine resistance in S. aureus (Costa et al., 2013; LaBreck et al., 2020). Exposure of S. mutans to chlorhexidine also yields cell wall damage that occurs on one hand, much faster than in S. aureus, but at the other hand is also rapidly self-repaired after exposure to chlorhexidine. As a result of this rapid self-repair, efflux of chlorhexidine is impossible leading to solidification of the cytoplasm (McDonnell and Russell, 1999) due to precipitation of proteins and nucleic acids. Therewith, self-repair becomes suicidal and prevents the development of a chlorhexidine-resistant progeny in S. mutans. In line, no increased metabolic activity was observed in S. mutans upon exposure to chlorhexidine. Importantly, the physicochemical surface properties relevant for adhesion (Figure 3) did not change upon chlorhexidine exposure for all the three strains and cannot be held accountable for the changes in cell wall deformation observed.

S. aureus and S. mutans are both the Gram-positive bacterial strains and both their cell walls are composed of an array of surface appendages, a relatively thick layer of peptidoglycan, and a lipid membrane. The relatively rigid peptidoglycan layer is designed to resist intracellular pressure and maintain cell shape (Dover et al., 2015). Cell shape is compromised by the adhesion forces a bacterium experiences when it adheres to a surface, which leads to nanoscopic deformation of the cell wall. When the adhesion force experienced equals the opposing elastic forces from the peptidoglycan layer and the intracellular pressure, cell wall deformation stabilizes (see Figure 1), as observed here (see Figure 2). Upon exposure to chlorhexidine, cell wall deformation increases in both the strains, indicative of cell wall damage and leakage of intracellular material (Gilbert and Moore, 2005) and therewith, a loss of intracellular pressure, leading to ongoing deformation unless the cell wall damage is rapidly self-repaired, as concluded here to occur in S. mutans demonstrating reversible cell wall deformation after chlorhexidine exposure (Figure 2C).

We here used surface-enhanced fluorescence as a measure for cell wall deformation. As an advantage of surface-enhanced fluorescence over microscopic (fluorescence based) techniques, it measures cell wall deformation over several millions of bacteria, while microscopic techniques yield visualization of the damage of only a couple of hundred bacteria at best, depending on the type of microscopy and magnification applied. Here, we employed fluorescence microscopy using propidium iodide to demonstrate that increased cell wall deformation included increased permeability of the cell membrane. The bacterial cell membrane is an integral part of the cell wall and becomes penetrable to propidium iodide when damaged (Lehtinen et al., 2004). Chlorhexidine is a positively-charged molecule known to damage the cell wall and destabilize the membrane by interacting with negatively-charged phospholipids to create membrane holes (McDonnell and Russell, 1999). Microscopic holes after chlorhexidine exposure have been found in both the Gram-positive and Gram-negative bacteria. The number of holes increased with exposure time to chlorhexidine and concentration (Cheung et al., 2012).

Once chlorhexidine-induced cell wall deformation has commenced, this can lead to a cascade of different events. Bacterial cell wall deformation enhances the surface area of the lipid bilayer membrane enveloping the cytoplasm. This affects the lipid bilayer tension in the membrane that can subsequently activate mechanosensitive proteins located in the cell wall (Harapanahalli et al., 2015; Laventie and Jenal, 2020). In S. aureus, mechanosensing due to cell wall deformation has been demonstrated to be involved in the gating of mechanosensitive transmembrane channels (Carniello et al., 2020) to regulate transport across the membrane and the activation of nisin efflux pumps (Carniello et al., 2018b). Clearly, this cascade of events in S. aureus is energy-consuming, as evidenced by the increased metabolic activity of S. aureus in presence of chlorhexidine (see Figure 6). Also, streptococcal membrane proteins have been suggested to be involved in membrane pumping (Lorca et al., 2007), but their possible activation by cell wall deformation has not yet been demonstrated. Likely, the membrane insertases YidC–Oxa1–Alb3 that function as signaling proteins and catalyze the synthesis of new membrane proteins are responsible for the rapid self-repair of cell wall damage inflicted by chlorhexidine in S. mutans (Suntharalingam et al., 2009; Dalbey et al., 2014). S. mutans has two YidCs of which YidC1 preferentially operates in the absence of signal recognition particle pathways and YidC2 being the preferred insertase in presence of signal recognition particle pathways (Vasquez et al., 2021). Possession of two YidC paralogs may be the reason for the rapid self-repair under chlorhexidine stress in S. mutans as compared with S. aureus possessing only the YidC2 paralog (Shahmirzadi et al., 2016). Self-repair impedes reduction of intracellular chlorhexidine concentration that may lead to lethal solidification of the cytoplasm. Simultaneous self-repair and death due to cytoplasm solidification (McDonnell and Russell, 1999; Cieplik et al., 2019) explain the low metabolic activity in S. mutans during exposure to chlorhexidine (see also Figure 6).

Subculturing in vitro of S. mutans in the presence of increasing concentrations of chlorhexidine up to 1.5 μg/ml can increase the MIC of S. mutans up to 3-fold to yield a more resistant variant (Kaspar et al., 2019). We, oppositely, found that repeated subculturing at 1.2 μg/ml and stepwise higher could not induce resistance. These two opposing results must be viewed with respect to the clinical observation that S. mutans resistance to chlorhexidine is extremely rare (Cieplik et al., 2019). Chlorhexidine does not distinguish itself from other oral antimicrobials such as cetylpyridinium chloride in its ability to kill bacteria at high concentrations (Renton-Harper et al., 1996). Rather, the ability of chlorhexidine to adsorb to oral tissues and its subsequent release over prolonged periods of time up to 12 h is the key to its success as a most effective oral antimicrobial. Prolonged release in the oral cavity after a 30–60 s rinse yields concentrations of chlorhexidine that critically varies above and below the concentrations applied in the study by Kaspar et al. (2019) and ours. This suggests that the response of S. mutans to chlorhexidine may critically depend on concentration (Cieplik et al., 2019). Although chlorhexidine concentrations in saliva hover around the concentrations used by Kaspar et al. (2019) and ours, it is likely that S. mutans encounters higher chlorhexidine concentrations than occurring in saliva as it adheres to salivary conditioning films that constitute a reservoir of absorbed and adsorbed chlorhexidine. Suicidal self-repair would, therewith, explain why chlorhexidine-resistant S. mutans have not been clinically found.

This study presents a new perspective on the question why clinically S. mutans has hardly shown any signs of resistance to chlorhexidine by comparing its response to chlorhexidine with the response of S. aureus. Suicidal self-repair of cell wall damage upon chlorhexidine exposure in S. mutans is essential in maintaining its susceptibility for chlorhexidine during the periods that low concentrations of chlorhexidine exist in the oral cavity. S. aureus lacks such an overly effective self-repair mechanisms and found ways for effective efflux of chlorhexidine that allowed it to develop chlorhexidine resistance.

Data Availability Statement

The original contributions presented in the study are included in the article/Supplementary Material, further inquiries can be directed to the corresponding author.

Author Contributions

ML and VS contributed to conception, design, data acquisition, analysis and interpretation, and drafted and critically revised the manuscript. GG-D, MD, and WW contributed to data acquisition, analysis and interpretation, and manuscript reviewing. VC contributed to data acquisition and critically revised the manuscript. HB, HM, and YR contributed to conception, design, data analysis and interpretation, and drafted and critically revised the manuscript. All authors gave final approval and agreed to be accountable for all the aspects of this study.

Funding

This study was supported by the University Medical Center Groningen-University of Groningen, Netherlands.

Author Disclaimer

Opinions and assertions contained herein are those of the authors and are not construed as necessarily representing views of the funding organization or their respective employer(s).

Conflict of Interest

HB was also director of a consulting company SASA BV, Thesinge, Netherlands.

The remaining authors declare that the research was conducted in the absence of any commercial or financial relationships that could be construed as a potential conflict of interest.

Publisher’s Note

All claims expressed in this article are solely those of the authors and do not necessarily represent those of their affiliated organizations, or those of the publisher, the editors and the reviewers. Any product that may be evaluated in this article, or claim that may be made by its manufacturer, is not guaranteed or endorsed by the publisher.

Acknowledgments

We would like to thank Deng from the Academic Center for Dentistry, Amsterdam, Netherlands for providing the green fluorescent S. mutans strain.

Supplementary Material

The Supplementary Material for this article can be found online at: https://www.frontiersin.org/articles/10.3389/fmicb.2022.861890/full#supplementary-material

References

Balagopal, S., and Arjunkumar, E. (2013). Chlorhexidine: the gold standard antiplaque agent. J. Pharmaceut. Sci. Res. 5, 270–274.

Google Scholar

Beyth, N., Redlich, M., Harari, D., Friedman, M., and Steinberg, D. (2003). Effect of sustained-release chlorhexidine varnish on Streptococcus mutans and Actinomyces viscosus in orthodontic patients. Am. J. Orthod. Dentofacial Orthop. 123, 345–348. doi: 10.1067/mod.2003.19

PubMed Abstract | CrossRef Full Text | Google Scholar

Block, C., and Furman, M. (2002). Association between intensity of chlorhexidine use and micro-organisms of reduced susceptibility in a hospital environment. J. Hosp. Infect. 51, 201–206. doi: 10.1053/jhin.2002.1246

PubMed Abstract | CrossRef Full Text | Google Scholar

Carniello, V., Peterson, B. W., Sjollema, J., Busscher, H. J., and Van der Mei, H. C. (2018a). Surface enhanced fluorescence and nanoscopic cell wall deformation in adhering Staphylococcus aureus upon exposure to cell wall active and non-active antibiotics. Nanoscale 10, 11123–11133. doi: 10.1039/c8nr01669k

PubMed Abstract | CrossRef Full Text | Google Scholar

Carniello, V., Harapanahalli, A. K., Busscher, H. J., and Van der Mei, H. C. (2018b). Adhesion force sensing and activation of a membrane-bound sensor to activate nisin efflux pumps in Staphylococcus aureus under mechanical and chemical stresses. J. Colloid Interface Sci. 512, 14–20. doi: 10.1016/j.jcis.2017.10.024

PubMed Abstract | CrossRef Full Text | Google Scholar

Carniello, V., Peterson, B. W., Van der Mei, H. C., and Busscher, H. J. (2020). Role of adhesion forces in mechanosensitive channel gating in Staphylococcus aureus adhering to surfaces. NPJ Biofilms Microbiomes 6:31. doi: 10.1038/s41522-020-00141-z

PubMed Abstract | CrossRef Full Text | Google Scholar

Cheung, H. Y., Wong, M. M. K., Cheung, S. H., Liang, L. Y., Lam, Y. W., and Chiu, S. K. (2012). Differential actions of chlorhexidine on the cell wall of Bacillus subtilis and Escherichia coli. PLoS One 7:e36659. doi: 10.1371/journal.pone.0036659

PubMed Abstract | CrossRef Full Text | Google Scholar

Cieplik, F., Jakubovics, N. S., Buchalia, W., Maisch, T., Hellwig, E., and Al-Ahmad, A. (2019). Resistance toward chlorhexidine in oral bacteria-is there cause for concern? Front. Microbiol. 10:587. doi: 10.3389/fmicb.2019.00587

PubMed Abstract | CrossRef Full Text | Google Scholar

Costa, S. S., Junqueira, E., Palma, C., Viveiros, M., Melo-Cristino, J., Amaral, L., et al. (2013). Resistance to antimicrobials mediated by efflux pumps in Staphylococcus aureus. Antibiotics 2, 83–99. doi: 10.3390/antibiotics2010083

PubMed Abstract | CrossRef Full Text | Google Scholar

Dalbey, R. E., Kuhn, A., Zhu, L., and Kiefer, D. (2014). The membrane insertase YidC. Biochim. Biophys. Acta 1843, 1489–1496. doi: 10.1016/j.bbamcr.2013.12.022

PubMed Abstract | CrossRef Full Text | Google Scholar

Deng, D. M., Ten Cate, J. M., and Crielaard, W. (2007). The adaptive response of Streptococcus mutans towards oral care products: involvement of the ClpP serine protease. Eur. J. Oral Sci. 115, 363–370. doi: 10.1111/j.1600-0722.2007.00477.x

PubMed Abstract | CrossRef Full Text | Google Scholar

Denton, G. W. (2001). “Chlorhexidine,” in Disinfection, Sterilization and Preservation, 5th Edn, ed. S. S. Block (Philadelphia: Lea and Febiger), 321–336.

Google Scholar

Dover, R. S., Bitler, A., Shimoni, E., Trieu-Cuot, P., and Shai, Y. (2015). Multiparametric AFM reveals turgor-responsive net-like peptidoglycan architecture in live streptococci. Nat. Commun. 6:7193. doi: 10.1038/ncomms8193

PubMed Abstract | CrossRef Full Text | Google Scholar

Gilbert, P., and Moore, L. E. (2005). Cationic antiseptics: diversity of action under a common epithet. J. Appl. Microbiol. 99, 703–715. doi: 10.1111/j.1365-2672.2005.02664.x

PubMed Abstract | CrossRef Full Text | Google Scholar

Harapanahalli, A. K., Younes, J. A., Allan, E., Van der Mei, H. C., and Busscher, H. J. (2015). Chemical signals and mechanosensing in bacterial responses to their environment. PLoS Pathog. 11:e1005057. doi: 10.1371/journal.ppat.1005057

PubMed Abstract | CrossRef Full Text | Google Scholar

Howard, D. H., Scott, R. D., Packard, R., and Jones, D. (2003). The global impact of drug resistance. Clin. Infect. Dis. 36, 4–10. doi: 10.1086/344656

PubMed Abstract | CrossRef Full Text | Google Scholar

Jutkina, J., Marathe, N. P., Flach, C. F., and Larsson, D. G. J. (2018). Antibiotics and common antibacterial biocides stimulate horizontal transfer of resistance at low concentrations. Sci. Total Environ. 616–617, 172–178. doi: 10.1016/j.scitotenv.2017.10.312

PubMed Abstract | CrossRef Full Text | Google Scholar

Kampf, G. (2016). Acquired resistance to chlorhexidine – it is time to establish an ‘antiseptic stewardship’ initiative? J. Hosp. Infect. 94, 213–227. doi: 10.1016/j.jhin.2016.08.018

PubMed Abstract | CrossRef Full Text | Google Scholar

Kaspar, J. R., Godwin, M. J., Velsko, I. M., Richards, V. P., and Burne, R. A. (2019). Spontaneously arising Streptococcus mutans variants with reduced susceptibility to chlorhexidine display genetic defects and diminished fitness. Antimicrob. Agents Chemother. 63, e00161–19. doi: 10.1128/AAC.00161-19

PubMed Abstract | CrossRef Full Text | Google Scholar

Krom, B. P., Cohen, J. B., McElhaney Feser, G. E., and Cihlar, R. L. (2007). Optimized candidal biofilm microtiter assay. J. Microbiol. Methods 68, 421–3. doi: 10.1016/j.mimet.2006.08.003

PubMed Abstract | CrossRef Full Text | Google Scholar

Kumar, S. B. (2017). Chlorhexidine mouthwash-a review. J. Pharmaceut. Sci. Res. 9, 1450–1452.

Google Scholar

LaBreck, P. T., Bochi-Layec, A. C., Stanbro, J., Dabbah-Krancher, G., Simons, M. P., and Merrell, D. S. (2020). Systematic analysis of efflux pump-mediated antiseptic resistance in Staphylococcus aureus suggests a need for greater antiseptic stewardship. mSphere 5, e00959–19. doi: 10.1128/mSphere.00959-19

PubMed Abstract | CrossRef Full Text | Google Scholar

Laventie, B.-J., and Jenal, U. (2020). Surface sensing and adaptation in bacteria. Ann. Rev. Microbiol. 74, 735–760. doi: 10.1146/annurev-micro-012120-063427

PubMed Abstract | CrossRef Full Text | Google Scholar

Lee, K., Hahn, L. D., Yuen, W. W., Vlamakis, H., Kolter, R., and Mooney, D. J. (2011). Metal-enhanced fluorescence to quality bacterial adhesion. Adv. Mat. 23, H101–H104. doi: 10.1002/adma.201004096

PubMed Abstract | CrossRef Full Text | Google Scholar

Lehtinen, J., Nuutila, J., and Lilius, E. M. (2004). Green fluorescent protein-propidium iodide (GFP-PI) based assay for flow cytometric measurement of bacterial viability. Cytometry A 60, 165–172. doi: 10.1002/cyto.a.20026

PubMed Abstract | CrossRef Full Text | Google Scholar

Li, J., Busscher, H. J., Swartjes, J., Chen, Y., Harapanahalli, A. K., Norde, W., et al. (2014). Residence-time dependent cell wall deformation of different Staphylococcus aureus strains on gold measured using surface-enhanced-fluorescence. Soft Matter 10, 7638–7646. doi: 10.1039/c4sm00584h

PubMed Abstract | CrossRef Full Text | Google Scholar

Li, J., Busscher, H. J., Van der Mei, H. C., Norde, W., Krom, B. P., and Sjollema, J. (2011). Analysis of the contribution of sedimentation to bacterial mass transport in a parallel plate flow chamber: part II: use of fluorescence imaging. Colloids Surf. B Biointerfaces 87, 427–432. doi: 10.1016/j.colsurfb.2011.06.002

PubMed Abstract | CrossRef Full Text | Google Scholar

Lichtenberg, D., Rosenberg, M., Sharfman, N., and Ofek, I. (1985). A kinetic approach to bacterial adherence to hydrocarbon. J. Microbiol. Methods 4, 141–146. doi: 10.1016/0167-7012(85)90029-6

CrossRef Full Text | Google Scholar

Loesche, W. J. (1986). Role of Streptococcus mutans in human dental decay. Microbiol. Rev. 50, 353–380. doi: 10.1128/mr.50.4.353-380.1986

PubMed Abstract | CrossRef Full Text | Google Scholar

Lorca, G. L., Barabote, R. D., Zlotopolski, V., Tran, C., Winnen, B., Hvorup, R. N., et al. (2007). Transport capabilities of eleven gram-positive bacteria: comparative genomic analyses. Biochim. Biophys. Acta 1768, 1342–1366. doi: 10.1016/j.bbamem.2007.02.007

PubMed Abstract | CrossRef Full Text | Google Scholar

McCormack, M. G., Smith, A. J., Akram, A. N., Jackson, M., Robertson, D., and Edwards, G. (2015). Staphylococcus aureus and the oral cavity: an overlooked source of carriage and infection? Am. J. Infect. Control 43, 35–37. doi: 10.1016/j.ajic.2014.09.015

PubMed Abstract | CrossRef Full Text | Google Scholar

McDonnell, G., and Russell, A. D. (1999). Antiseptics and disinfectants: activity, action, and resistance. Clin. Microbiol. Rev. 12, 147–179. doi: 10.1128/CMR.12.1.147

PubMed Abstract | CrossRef Full Text | Google Scholar

Nde, C. W., Jang, H. J., Toghrol, F., and Bentley, W. E. (2009). Global transcriptomic response of Pseudomonas aeruginosa to chlorhexidine diacetate. Environ. Sci. Technol. 43, 8406–8415. doi: 10.1021/es9015475

PubMed Abstract | CrossRef Full Text | Google Scholar

O’Neill, J. (2014). Antimicrobial Resistance: Tackling a Crisis for the Health and Wealth of Nations. Review on Antimicrobial Resistance. London: Review on Antimicrobial Resistance.

Google Scholar

Okada, E. M., Ribeiro, L. N., Stuani, M. B., Borsatto, M. C., da Silva Fidalgo, T. K., Garcia de Paula-Silva, F. W., et al. (2016). Effects of chlorhexidine varnish on caries during orthodontic treatment: a systematic review and meta-analysis. Braz. Oral Res. 30:e115. doi: 10.1590/1807-3107BOR-2016.vol30.0115

PubMed Abstract | CrossRef Full Text | Google Scholar

Reda, B., Hollemeyer, K., Trautmann, S., Volmer, D. A., and Hannig, M. (2021). First insights into chlorhexidine retention in the oral cavity after application of different regimens. Clin. Oral Invest. 25, 6109–6118. doi: 10.1007/s00784-021-03910-y

PubMed Abstract | CrossRef Full Text | Google Scholar

Renton-Harper, P., Addy, M., Moran, J., Doherty, F. M., and Newcombe, R. G. (1996). A comparison of chlorhexidine, cetylperidinium chloride, triclosan, and C13G mouthrinse products for plaque inhibition. J. Periodontol. 67, 486–489. doi: 10.1902/jop.1996.67.5.486

PubMed Abstract | CrossRef Full Text | Google Scholar

Roca, I., Akova, M., Baquero, F., Carlet, J., Cavaleri, M., Coenen, S., et al. (2015). The global threat of antimicrobial resistance: science for intervention. New Microbes New Infect. 6, 22–29. doi: 10.1016/j.nmni.2015.02.007

PubMed Abstract | CrossRef Full Text | Google Scholar

Saleem, H. G., Seers, C. A., Sabri, A. N., and Reynolds, E. C. (2016). Dental plaque bacteria with reduced susceptibility to chlorhexidine are multidrug resistant. BMC Microbiol. 16:214. doi: 10.1186/s12866-016-0833-1

PubMed Abstract | CrossRef Full Text | Google Scholar

Schlett, C. D., Millar, E. V., Crawford, K. B., Cui, T., Lanier, J. B., Tribble, D. R., et al. (2014). Prevalence of chlorhexidine-resistant methicillin-resistant Staphylococcus aureus following prolonged exposure. Antimicrob. Agents Chemother. 58, 4404–4410. doi: 10.1128/AAC.02419-14

PubMed Abstract | CrossRef Full Text | Google Scholar

Shahmirzadi, S. V., Nguyen, M. T., and Gotz, F. (2016). Evaluation of Staphylococcus aureus lipoproteins: role in nutritional acquisition and pathogenicity. Front. Microbiol. 7:1404. doi: 10.3389/fmicb.2016.01404

PubMed Abstract | CrossRef Full Text | Google Scholar

Suntharalingam, P., Senadheera, M. D., Mair, R. W., Levesque, C. M., and Cvitkovitch, D. G. (2009). The LiaFSR system regulates the cell envelope stress response in Streptococcus mutans. J. Bacteriol. 191, 2973–2984. doi: 10.1128/JB.01563-08

PubMed Abstract | CrossRef Full Text | Google Scholar

Van der Wal, A., Minor, M., Norde, W., Zehnder, A. J. B., and Lylkema, J. (1997). Electrokinetic potential of bacterial cells. Langmuir 13, 165–171. doi: 10.1021/la960386k

CrossRef Full Text | Google Scholar

Vasquez, P. L., Mishra, S., Kuppuswamy, S. K., Crwoley, P. J., and Brady, L. J. (2021). Protein interactomes of Streptococcus mutans YidC1 and YidC2 membrane protein insertases suggest SRP pathway-independent- and -dependent functions, respectively. mSphere 6, e01308–20. doi: 10.1128/mSphere.01308-20

PubMed Abstract | CrossRef Full Text | Google Scholar

World Health Organization [WHO] (2018). World Health Organization [2018 Feb 2018; 2019 Jan 19]. Available online at: https://www.who.int/news-room/fact-sheets/detail/antibiotic-resistance (accessed February, 2018).

Google Scholar

Zaura-Arite, E., Van Marle, J., and Ten Cate, J. M. (2001). Confocal microscopy study of undisturbed and chlorhexidine-treated dental biofilm. J. Dent. Res. 80, 1436–1440. doi: 10.1177/00220345010800051001

PubMed Abstract | CrossRef Full Text | Google Scholar

Zhang, T. T., Tang, S. S., and Fu, L. J. (2013). The effectiveness of different concentrations of chlorhexidine for prevention of ventilator-associated pneumonia: a meta-analysis. J. Clin. Nurs. 23, 1461–1475. doi: 10.1111/jocn.12312

PubMed Abstract | CrossRef Full Text | Google Scholar

Zuttion, F., Colom, A., Matile, S., Farago, D., Pompeo, F., Kokavecz, J., et al. (2020). High-speed atomic force microscopy highlights new molecular mechanism daptomycin action. Nat. Commun. 11:6312. doi: 10.1038/s41467-020-19710-z

PubMed Abstract | CrossRef Full Text | Google Scholar

Keywords: self-repair, antimicrobials, cell wall deformation, cell wall damage, solidification of cytoplasm, resistance

Citation: van de Lagemaat M, Stockbroekx V, Geertsema-Doornbusch GI, Dijk M, Carniello V, Woudstra W, van der Mei HC, Busscher HJ and Ren Y (2022) A Comparison of the Adaptive Response of Staphylococcus aureus vs. Streptococcus mutans and the Development of Chlorhexidine Resistance. Front. Microbiol. 13:861890. doi: 10.3389/fmicb.2022.861890

Received: 25 January 2022; Accepted: 11 April 2022;
Published: 19 May 2022.

Edited by:

Nelson da Cruz Soares, University of Sharjah, United Arab Emirates

Reviewed by:

Mohamad Hamad, University of Sharjah, United Arab Emirates
Suereta Fortuin, Stellenbosch University, South Africa
Abiola Senok, Mohammed Bin Rashid University of Medicine and Health Sciences, United Arab Emirates

Copyright © 2022 van de Lagemaat, Stockbroekx, Geertsema-Doornbusch, Dijk, Carniello, Woudstra, van der Mei, Busscher and Ren. This is an open-access article distributed under the terms of the Creative Commons Attribution License (CC BY). The use, distribution or reproduction in other forums is permitted, provided the original author(s) and the copyright owner(s) are credited and that the original publication in this journal is cited, in accordance with accepted academic practice. No use, distribution or reproduction is permitted which does not comply with these terms.

*Correspondence: Henny C. van der Mei, aC5jLnZhbi5kZXIubWVpQHVtY2cubmw=

These authors have contributed equally to this work

Disclaimer: All claims expressed in this article are solely those of the authors and do not necessarily represent those of their affiliated organizations, or those of the publisher, the editors and the reviewers. Any product that may be evaluated in this article or claim that may be made by its manufacturer is not guaranteed or endorsed by the publisher.